Tin

Density

7310 kg/m3

Melting Point

232 °C

Thermal Conductivity

67 W / °C

Electrical Conductivity

0,91 ·10⁷ S/M

Hardness

1,5 Mohs

Modulus of elasticity

50 GPa

Thermal Expansion

22 ∙ 10-6 m / K

Description